Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 85 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.16 g/cc
0.331 lb/in³
Thermal Properties Metric English Comments
Melting Point 96.0 - 143 °C
205 - 289 °F
Solidus 96.0 °C
205 °F
Liquidus 143 °C
289 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 33.4 %
33.4 %
Lead, Pb 33.3 %
33.3 %
Tin, Sn 33.3 %
33.3 %