Thermal Properties Metric English Comments
Liquidus 157 °C
315 °F
Indium Corp. Indalloy® 4 Pure Indium Solder
Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni..
Liquidus 157 °C
315 °F
Williams Advanced Alloys WS157 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys