Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 187 °C | 369 °F | |
Indium Corp. Indalloy 226 Tin Solder Alloy Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation |
|||
Liquidus | 187 °C | 369 °F | |
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut.. |
|||
Liquidus | 187 °C | 369 °F | |
Williams Advanced Alloys WS187 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |