Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1530 °C | 2790 °F | |
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
Liquidus | 1530 °C | 2790 °F | |
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
Liquidus | 1530 °C | 2790 °F | |
CMW® D57F Silver Iron Contact Material For electrical contacts; AC resistive loads.Information provided by CMW Inc. |
|||
Liquidus | 1532 °C | 2790 °F | |
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
Liquidus | 1532 °C | 2790 °F | |
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Liquidus | 1530 °C | 2790 °F | |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Liquidus | 1532 °C | 2790 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |