Material Notes:
Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Specific Gravity 7.70 g/cc
7.70 g/cc
Mechanical Properties Metric English Comments
Hardness, Brinell 155
155
Tensile Strength, Ultimate 517 MPa
75000 psi
Tensile Strength, Yield 310 MPa

@Strain 0.200 %
45000 psi

@Strain 0.200 %
Elongation at Break 30 %
30 %
in 2"
Reduction of Area 75 %
75 %
Modulus of Elasticity 200 GPa
29000 ksi
Tension
Poissons Ratio 0.32
0.32
Calculated
Shear Modulus 75.8 GPa
11000 ksi
Izod Impact Unnotched 122 J
90.0 ft-lb
Thermal Properties Metric English Comments
CTE, linear 9.90 µm/m-°C

@Temperature 0.000 - 100 °C
5.50 µin/in-°F

@Temperature 32.0 - 212 °F
10.1 µm/m-°C

@Temperature 0.000 - 316 °C
5.60 µin/in-°F

@Temperature 32.0 - 600 °F
11.7 µm/m-°C

@Temperature 0.000 - 649 °C
6.50 µin/in-°F

@Temperature 32.0 - 1200 °F
Thermal Conductivity 24.90 W/m-K

@Temperature 93.3 °C
172.8 BTU-in/hr-ft²-°F

@Temperature 200 °F
28.5 W/m-K

@Temperature 538 °C
198 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Melting Point 1480 - 1530 °C
2700 - 2790 °F
Solidus 1480 °C
2700 °F
Liquidus 1530 °C
2790 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 11.5 - 13.5 %
11.5 - 13.5 %
Iron, Fe >= 84.28 %
>= 84.28 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000569 ohm-cm

@Temperature 23.0 °C
0.0000569 ohm-cm

@Temperature 73.4 °F
Descriptive Properties Value Comments
Endurance Limit, ksi 40