Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 186 °C | 367 °F | |
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy Pb free solder. Zn causes high drossing; corrosion concerns.Information provided by the manufacturer, Indium Corporation. |
|||
Liquidus | 186 °C | 367 °F | |
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy Good pre-tinning alloyInformation Provided by Indium Corporation |
|||
Liquidus | 186 °C | 367 °F | |
Williams Advanced Alloys WS186 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |