Polymer Property : Liquidus = 437 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 225 °C
437 °F
Indium Corp. Indalloy 251 Tin Solder Alloy
Castin Patented alloyInformation Provided by Indium Corporation
Liquidus 225 °C
437 °F
Johnson Matthey Plumbsol Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..
Liquidus 225 °C
437 °F
Lucas-Milhaupt Silvabrite® Lead-Free Solder
Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl..
Liquidus 225 °C
437 °F
Williams Advanced Alloys WS225 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Liquidus 225 °C
437 °F
AIM 40In/60Pb Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.