AIM 40In/60Pb Solder for Photonic Packaging

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer AIM Specialty Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AIM 40In/60Pb Solder for Photonic Packaging.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Physical Properties Metric English Comments
Density 9.31 g/cc
0.336 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 238 MPa
34500 psi
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
Melting Point 195 - 225 °C
383 - 437 °F
Solidus 195 °C
383 °F
Liquidus 225 °C
437 °F
Component Elements Properties Metric English Comments
Indium, In 40 %
40 %
Lead, Pb 60 %
60 %
Descriptive Properties Value Comments
Creep Resistance Moderate