Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 688 °C
1270 °F
Flow Point
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal
Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter..
Liquidus 688 °C
1270 °F
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu..
Liquidus 688 °C
1270 °F
Flow Point
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy
Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi..
Liquidus 688 °C
1270 °F
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy
Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos..
Liquidus 688 °C
1270 °F
Universal Wire Works BAg-3 (AMS 4771) Silver Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.