Polymer Property : Hot Ball Pressure Test = 129 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 129 °C
<= 264 °F
IEC 60695-10-2
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East)
XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.