Polymer Property : Hot Ball Pressure Test = 210 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Hot Ball Pressure Test 210 °C
410 °F
IEC 60695-10-2
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Hot Ball Pressure Test 210 °C

@Thickness 3.00 mm
410 °F

@Thickness 0.118 in
IEC 60695-10-2
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym..
Hot Ball Pressure Test 210 °C

@Thickness 3.00 mm
410 °F

@Thickness 0.118 in
IEC 60695-10-2
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded
Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym..