Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 80.0 °C
<= 176 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East)
CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri..
Hot Ball Pressure Test <= 80.0 °C
<= 176 °F
IEC 60695-10-2
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications.
Hot Ball Pressure Test 80.0 - 105 °C
176 - 221 °F
Average value: 95.0 °C Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Hot Ball Pressure Test 80.0 - 100 °C
176 - 212 °F
Average value: 94.5 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Hot Ball Pressure Test 80.0 °C

@Thickness 2.00 mm
176 °F

@Thickness 0.0787 in
IEC695-10-2
Kingfa FRHIPS-1162 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl..
Hot Ball Pressure Test <= 80.0 °C
<= 176 °F
IEC 60695-10-2
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East)
NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat..
Hot Ball Pressure Test 80.0 °C

@Thickness 2.00 mm
176 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Sax Polymers SAXATEC 6120 AES
SAXATEC 6120 is a easy lowing, weatherable AES injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym..
Hot Ball Pressure Test 80.0 °C

@Thickness 2.00 mm
176 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene
Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided..
Hot Ball Pressure Test 80.0 °C
176 °F
JET, 2.0 mm
Total PSI 3341 High Impact Polystyrene
Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri..
Hot Ball Pressure Test >= 80.0 °C
>= 176 °F
BS 3456, IEC 335
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene
Hot Ball Pressure Test >= 80.0 °C
>= 176 °F
BS 3456, IEC 335
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber
Characteristics: 10% glass fibre filled
Hot Ball Pressure Test >= 80.0 °C
>= 176 °F
BS 3456, IEC 335
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled