Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Hot Ball Pressure Test 98.0 °C

@Thickness 2.00 mm
208 °F

@Thickness 0.0787 in
IE/CEN 60335-1
Sax Polymers SAXLAC 108 GF17 Acrylonitrile Butadiene Styrene, 17% Glass Fiber
Saxalac 108 GF17 is a 17% glass fiber reinforced ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data te..
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Hot Ball Pressure Test <= 98.0 °C
<= 208 °F
IEC 60695-10-2
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.