Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature <=162 °C
5.56 µin/in-°F

@Temperature <=324 °F
Below Tg; ISO 11359
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® BR42B 40% glass fiber reinforced polyphenylene sulfide compound is specially formulated to provide low coefficient of friction and reduced wear rate for use in applications requiring low s..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2; ISO 11359-2
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2; ISO 11359-2
Solvay Specialty Polymers Ryton® R-4-280NA Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280NA 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled
Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S..
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta..
Copyright © lookpolymers.com All Rights Reserved