Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 150 - 250 °C
6.11 µin/in-°F

@Temperature 302 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 150 - 250 °C
6.11 µin/in-°F

@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material ..
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 160 - 250 °C
6.11 µin/in-°F

@Temperature 320 - 482 °F
2
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
6.11 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 75-1/-2
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 160 - 249 °C
6.11 µin/in-°F

@Temperature 320 - 480 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 100 - 200 °C
6.11 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..