Polymer Property : CTE, linear, Parallel to Flow = 11.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -20.0 - 150 °C
11.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR48 PBT
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature 60.0 - 138 °C
11.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR48 PBT
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature 60.0 - 138 °C
11.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature 60.0 - 138 °C
11.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific)
LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS
LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural.