Polymer Property : CTE, linear, Parallel to Flow = 17.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 0.000 - 100 °C
17.2 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 200 - 250 °C
17.2 µin/in-°F

@Temperature 392 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 50.0 - 100 °C
17.2 µin/in-°F

@Temperature 122 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 0.000 - 100 °C
17.2 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 200 - 250 °C
17.2 µin/in-°F

@Temperature 392 - 482 °F
4
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral
Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 50.0 - 100 °C
17.2 µin/in-°F

@Temperature 122 - 212 °F
4
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral
Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over..
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU
LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU
LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 30.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
CTE, linear, Parallel to Flow 30.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
CTE, linear, Parallel to Flow 30.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.