Polymer Property : CTE, linear, Parallel to Flow = 171 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature -40.0 - 40.0 °C
95.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature -40.0 - 40.0 °C
95.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp FX00617 PE
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature -40.0 - 40.0 °C
95.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..
CTE, linear, Parallel to Flow 171 µm/m-°C

@Temperature -40.0 - 40.0 °C
95.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific)
LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia..