Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 171 µm/m-°C @Temperature -40.0 - 40.0 °C |
95.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
CTE, linear, Parallel to Flow | 171 µm/m-°C @Temperature -40.0 - 40.0 °C |
95.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
CTE, linear, Parallel to Flow | 171 µm/m-°C @Temperature -40.0 - 40.0 °C |
95.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
CTE, linear, Parallel to Flow | 171 µm/m-°C @Temperature -40.0 - 40.0 °C |
95.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |