Polymer Property : CTE, linear, Parallel to Flow = 20.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI
LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific)
LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
CTE, linear, Parallel to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.