Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 61.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
CTE, linear, Parallel to Flow | 61.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
CTE, linear, Parallel to Flow | 61.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
CTE, linear, Parallel to Flow | 61.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
CTE, linear, Parallel to Flow | 61.5 µm/m-°C @Temperature -40.0 - 60.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
CTE, linear, Parallel to Flow | 61.5 µm/m-°C @Temperature -40.0 - 60.0 °C |
34.2 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |