Polymer Property : CTE, linear, Parallel to Flow = 61.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp DFI12E PC
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific)
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature 60.0 - 138 °C
34.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 855 PBT
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature 60.0 - 138 °C
34.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific)
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -30.0 - 30.0 °C
34.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East)
DATA ON BK1005 ONLY.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -30.0 - 30.0 °C
34.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS
DATA ON BK1005 ONLY.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC
design for black light frame application as high flow PC, V-2, high reflection grade.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific)
design for black light frame application as high flow PC, V-2, high reflection grade.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East)
design for black light frame application as high flow PC, V-2, high reflection grade.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific)
LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP
LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
CTE, linear, Parallel to Flow 61.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
34.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp GL004 PSU
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re..