Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 160 - 250 °C |
55.6 µin/in-°F @Temperature 320 - 482 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 100 - 150 °C |
55.6 µin/in-°F @Temperature 212 - 302 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 100 - 150 °C |
55.6 µin/in-°F @Temperature 212 - 302 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 95.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -30.0 - 80.0 °C |
55.6 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 55.0 - 160 °C |
55.6 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature 100 - 200 °C |
55.6 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t.. |
|||
CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |