Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific)
LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
CTE, linear, Transverse to Flow 32.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp EC002E PEI
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific)
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE0049P PC
LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct..