SABIC Innovative Plastics LNP STAT-KON EX99689C PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON EX99689C PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Moisture Absorption 0.300 %
0.300 %
50% RH, 24 hrs; ASTM D570
0.350 %
0.350 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0017 cm/cm

@Time 86400 sec
0.0017 in/in

@Time 24.0 hour
ISO 294
0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0036 cm/cm

@Time 86400 sec
0.0036 in/in

@Time 24.0 hour
ISO 294
0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 137 MPa
19900 psi
ISO 527
161 MPa
23400 psi
ASTM D638
Elongation at Break 1.2 %
1.2 %
ISO 527
1.6 %
1.6 %
ASTM D638
Tensile Modulus 11.65 GPa
1690 ksi
50 mm/min; ASTM D638
12.63 GPa
1832 ksi
1 mm/min; ISO 527
Flexural Strength 216 MPa
31300 psi
ISO 178
241 MPa
35000 psi
ASTM D790
Flexural Modulus 10.31 GPa
1495 ksi
ISO 178
10.8 GPa
1570 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.48 J/cm
8.39 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 11.0 J
8.11 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 33.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
33.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 32.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
33.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.350 mm
V-0

@Thickness 0.0138 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257