Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 46.0 µm/m-°C @Temperature 0.000 - 100 °C |
25.6 µin/in-°F @Temperature 32.0 - 212 °F |
|
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |