Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
CTE, linear, Transverse to Flow | 69.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |