Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare
CTE, linear, Transverse to Flow 69.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare