Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
CTE, linear, Transverse to Flow | 70.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 70.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 70.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 71.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66