Polymer Property : CTE, linear, Transverse to Flow = 41.5 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer
Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer
LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.