Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
1.40 g/cc
0.0506 lb/in³
ASTM D792
Moisture Absorption 0.870 %
0.870 %
50% RH, 24 hrs; ASTM D570
1.07 %
1.07 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0029 cm/cm

@Time 86400 sec
0.0029 in/in

@Time 24.0 hour
ISO 294
0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm

@Time 86400 sec
0.0090 - 0.011 in/in

@Time 24.0 hour
ASTM D955
0.010 cm/cm

@Time 86400 sec
0.010 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
ASTM D638
140 MPa
20300 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ASTM D638
2.6 %
2.6 %
ISO 527
Tensile Modulus 9.40 GPa
1360 ksi
1 mm/min; ISO 527
9.85 GPa
1430 ksi
50 mm/min; ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
217 MPa
31500 psi
ISO 178
Flexural Modulus 7.44 GPa
1080 ksi
ASTM D790
8.90 GPa
1290 ksi
ISO 178
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.31 J/cm
13.7 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 46.0 kJ/m²
21.9 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 26.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
29.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 74.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
74.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 252 °C

@Thickness 3.20 mm
486 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
230 °C

@Thickness 3.20 mm
446 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94 by SABIC-IP
Users viewing this material also viewed the following: