Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific)
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC
LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66
LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific)
LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS
LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific)
LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific)
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific)
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66
LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific)
LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66
LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT
LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific)
LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp MX88073 PP
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific)
LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS