Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 °C
26.1 µin/in-°F

@Temperature 73.4 °F
ASTM D696
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 200 °C
26.1 µin/in-°F

@Temperature 392 °F
ASTM D696
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 150 °C
26.1 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 150 °C
26.1 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 150 °C
26.1 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature 23.0 - 150 °C
26.1 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MFD03 PP
LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 47.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific)
LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.