Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12
LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12
LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific)
LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific)
LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific)
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature 23.0 - 55.0 °C
60.0 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature 23.0 - 55.0 °C
60.0 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers