Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
37.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 23.0 - 150 °C |
37.2 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature 200 - 300 °C |
37.2 µin/in-°F @Temperature 392 - 572 °F |
DIN 53 752 |
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
37.2 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |