Polymer Property : CTE, linear, Transverse to Flow = 7.20 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP
LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 7.20 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific)
LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa..