Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 945ASR PC
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp CI001 PS
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific)
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific)
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC
LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC
LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC
LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 1760 PBT+PC
11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature 25.6 - 93.3 °C
41.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10
LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific)
LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa..
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..