Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene641 Grade Bearing/Seal PTFE: FDA compliant, this formulation was specifically developed for food and drug applications. Rulon 641 is designed to run dry without any external lubrication and is compatible with 303 and 316 stainless steel mating surfaces. Rulon 641's high temperature and low wear properties offer major advantages as compared to other competitive FDA bearing materials, such as UHMWPE (Limited temperature tolerance and low load capacity at elevated temperatures) and virgin PTFE (Unacceptable wear properties and low load capacity at elevated temperatures). Rulon 641 is available in standard bearing sizes from 1/8" to 3" ID's White in color.Suitable for use in environments of steam, wet, dry, vacuum, or FDA type. Mating surface of 25 Rc or harder Steel. Material has electrical and thermal insulation properties. Markets for 641 grade include Appliances, Automotive, Dairy/Food/Beverage, Industrial, Medical, Transportation.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 2.25 g/cc
0.0813 lb/in³
ASTM D792
Water Absorption 0.00 %

@Time 86400 sec
0.00 %

@Time 24.0 hour
Immersion
Water Absorption at Saturation 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 175 %
175 %
ASTM D638
Compressive Yield Strength 6.89 MPa
1000 psi
Max load under tribological use
Coefficient of Friction, Dynamic 0.10 - 0.30
0.10 - 0.30
Dry vs. Steel
Coefficient of Friction, Static 0.10 - 0.30
0.10 - 0.30
Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec
10000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 99.0 µm/m-°C

@Temperature 25.6 - 93.3 °C
55.0 µin/in-°F

@Temperature 78.0 - 200 °F
Length
112 µm/m-°C

@Temperature 25.6 - 149 °C
62.0 µin/in-°F

@Temperature 78.0 - 300 °F
Length
CTE, linear, Transverse to Flow 73.8 µm/m-°C

@Temperature 25.6 - 93.3 °C
41.0 µin/in-°F

@Temperature 78.0 - 200 °F
Diameter
86.4 µm/m-°C

@Temperature 25.6 - 149 °C
48.0 µin/in-°F

@Temperature 78.0 - 300 °F
Diameter
Thermal Conductivity 0.375 W/m-K
2.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved