Polymer Property : CTE, linear, Transverse to Flow = 92.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 160 - 250 °C
51.1 µin/in-°F

@Temperature 320 - 482 °F
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such ..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
ASTM E 831
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 100 - 200 °C
51.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy  (discontinued **)
Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
CTE, linear, Transverse to Flow 92.0 µm/m-°C

@Temperature 100 - 200 °C
51.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy  (discontinued **)
Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with ..