Thermal Properties Metric English Comments
Heat Distortion Temperature 81.7 °C
179 °F
BCC Products METAL-KAST BC 8010 Urethane Casting
New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to..