Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75A |
Lucite International Diakon® CLG902L Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75A |
Lucite International Diakon® CLG902LX Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75A |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75A |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |
|||
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75A |
Lucite International Diakon® ST25H8 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Heat Distortion Temperature | 97.0 °C | 207 °F | ISO 75-2 |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |