Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 118000 J/g @Temperature 250 °C |
50800 BTU/lb @Temperature 482 °F |
|
Dow Corning 705 DIFFUSION PUMP FLUID A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning |