Polymer Property : Heat of Vaporization = 27.0 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 62.8 J/g

@Temperature 200 °C
27.0 BTU/lb

@Temperature 392 °F
at boiling point
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Heat of Vaporization 62.8 J/g

@Temperature 270 °C
27.0 BTU/lb

@Temperature 518 °F
at boiling point
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..