Thermal Properties Metric English Comments
Specific Heat Capacity 1.73 J/g-°C

@Temperature 200 °C
0.413 BTU/lb-°F

@Temperature 392 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Specific Heat Capacity 1.73 J/g-°C

@Temperature 200 °C
0.413 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..