Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.974 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.974 J/g-°C

@Temperature 100 °C
0.233 BTU/lb-°F

@Temperature 212 °F
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1..
Specific Heat Capacity 0.974 J/g-°C

@Temperature 100 °C
0.233 BTU/lb-°F

@Temperature 212 °F
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer
A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties...
Specific Heat Capacity 0.974 J/g-°C

@Temperature 100 °C
0.233 BTU/lb-°F

@Temperature 212 °F
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer
A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen..
Specific Heat Capacity 0.974 J/g-°C

@Temperature 100 °C
0.233 BTU/lb-°F

@Temperature 212 °F
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..