Specific Heat Capacity 1.04 J/g-°C

@Temperature 600 °C
0.249 BTU/lb-°F

@Temperature 1110 °F
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1”) upwards. F..
Specific Heat Capacity 1.04 J/g-°C

@Temperature -60.0 °C
0.249 BTU/lb-°F

@Temperature -76.0 °F
3M Novec™ 7000 Engineered Fluid
3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a..