Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 1.28 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.28 J/g-°C

@Temperature 50.0 °C
0.306 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
Specific Heat Capacity 1.28 J/g-°C

@Temperature 50.0 °C
0.306 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Specific Heat Capacity 1.28 J/g-°C

@Temperature 50.0 °C
0.306 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Specific Heat Capacity 1.28 J/g-°C

@Temperature 50.0 °C
0.306 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..