Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.66 J/g-°C @Temperature 200 °C |
0.397 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Specific Heat Capacity | 1.66 J/g-°C @Temperature 200 °C |
0.397 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Specific Heat Capacity | 1.66 J/g-°C @Temperature 200 °C |
0.397 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Specific Heat Capacity | 1.66 J/g-°C @Temperature 200 °C |
0.397 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |