Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET F096H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET F096HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET F097H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
|
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 0.000 °C |
0.436 BTU/lb-°F @Temperature 32.0 °F |
|
ChevronTexaco 22 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |
|||
Specific Heat Capacity | 1.82 J/g-°C @Temperature 200 °C |
0.435 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |