Thermal Properties Metric English Comments
Specific Heat Capacity 1.92 J/g-°C

@Temperature 23.9 °C
0.460 BTU/lb-°F

@Temperature 75.0 °F
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i..
Specific Heat Capacity 1.92 J/g-°C

@Temperature 100 °C
0.460 BTU/lb-°F

@Temperature 212 °F
DSC
Eastman Tritan FX200 Copolyester
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..